Used For
Stone, Recycled Bricks
Benefits- Increased bond strength over standard mortars makes a stickier brew
- Will assist in exceeding the masonry to mortar bond strength requirement of minimum 200kPa after 7 days for recycled bricks
- Technical and testing assistance available upon request
- Minimises waste
- Has consistent material calculations from bag to bag
- Contains a dry plasticiser accepted and endorsed by key trade users
- Can be coloured with Oxitone® oxides
- Trade Mortar Xtra is formulated to meet NZS4210:2001 Masonry Construction: Materials and Workmanship of 12.5MPa after 28 days (under standard curing conditions)